| Product Type | Raw Material |
|---|---|
| Product Categories | ABS |
| CAS NO. | 9003-56-9 |
| Manufacturers | INEOS |
| Grade | E112LG |
| Place of Origin | United Kingdom |
| Appearance | Natural |
| Packing Size | 25/KG Standard Packaging |
| Import | YES |
| Usage level | Car Parts, General Grade |
| Feature level | High Impact Resistance |
| Processing Method | Injection Molding |
| Shape | Particle |
Lustran® E112LG resin is a low-gloss, medium-impact extrusion grade of ABS (acrylonitrile butadiene styrene).
It has good melt strength for extrusion and thermoforming, and can be easily coextruded. It is easy to color with ABS color concentrates.
Motor vehicle dashboards
Interior panels and trim
Recreational vehicles, cars, trucks, construction vehicles, forklifts and farm equipment
| Test Method | ISO 1133 |
|---|---|
| Test Condition | 220℃ 10kg |
| Test Unit | cm³/10min |
| Test Result | 7 |
| Test Method | ISO 179/1eA |
|---|---|
| Test Condition | - |
| Test Unit | kJ/m² |
| Test Result | 11 |
| Test Method | ISO 179/1eA |
|---|---|
| Test Condition | - |
| Test Unit | kJ/m² |
| Test Result | 10 |
| Test Method | ISO 179/1eA |
|---|---|
| Test Condition | - |
| Test Unit | kJ/m² |
| Test Result | 9 |
| Test Method | ISO 527 |
|---|---|
| Test Condition | - |
| Test Unit | MPa |
| Test Result | 28 |
| Test Method | ISO 527 |
|---|---|
| Test Condition | - |
| Test Unit | % |
| Test Result | 2.9 |
| Test Method | ISO 527 |
|---|---|
| Test Condition | - |
| Test Unit | MPa |
| Test Result | 32 |
| Test Method | ISO 527 |
|---|---|
| Test Condition | - |
| Test Unit | % |
| Test Result | 75 |
| Test Method | ISO 527 |
|---|---|
| Test Condition | - |
| Test Unit | MPa |
| Test Result | 1600 |
| Test Method | ISO 306 |
|---|---|
| Test Condition | - |
| Test Unit | ℃ |
| Test Result | 95 |
| Test Method | - |
|---|---|
| Test Condition | - |
| Test Unit | - |
| Test Result | < 10 |
| Test Method | ISO 1183 |
|---|---|
| Test Condition | - |
| Test Unit | kg/m³ |
| Test Result | 1.04 |